Time Reheat Average Time Between Reheats Talia 27:50 26 Roughly one minute Hazel 55:19 25 roughly two minutes Sebass 41:01 18 roughly two minutes We also began to make a washer at the end of our time, but we created what was called “art”, in other words we got the tool stuck in the iron…
During the wool and dying process, our lab was focused far more on experimental qualitative data than the quantitative data often collected during the labs. However, we were able to quantify some of the process. Firstly, our dying results: We used woad seeds in a 2:1 ratio with the wool yarn. Thus: 100.2 grams of…